Products : Stainless Steel Seamless Pipe
Grade : S32760
Diameter : DN10 - DN400
Length : 6m or custom cutting any length as request
Standard : ASTM EN
Service : Cutting
Loading Port : Shanghai Port
Thickness : 4.0 - 50.0mm
S32760 (1.4501) Super Duplex Pipe With Excellent Pitting and Stress Corrosion Cracking Resistance
Products Specification
| Products Name | s32760 Duplex Stainless Steel Seamless Pipe |
Grade: | 304 304L 309S 310S 314 316L 316Ti 321 329 347H 410 2205 2507 S32760 904L 254SMO and equal grade in GB JIS EN DIN Standard |
| Standards: | ASTM A213M-94b ASTM A249M-94a ASTM A269-94a ASTM A312M-94b,ect. |
| DIN 17456-85 DIN 17458-85 DIN 17459-92.ect | |
| JIS G3446-1994 JIS G3448-1997 JIS G3459-1997 JIS G3463-1994,ect. | |
| GB13296-1991 GB14975-2002 GB14976-2002,ect. | |
| Size: | ND5 - DN400 |
| Length: | 6m length or cutting any length as request |
| Applications: | fluid and gas transport, structure , boiler, heat exchanger, super heater |
| Property | S32760 | 316L Austenitic | 2205 Duplex |
|---|---|---|---|
| PREN | 42–45 | 28–30 | 32–34 |
| Yield Strength | 550 MPa+ | 205 MPa | 450 MPa |
| H₂S Resistance | Excellent | Limited | Good |
| Cost Factor | 3.5x 316L | 1x | 2x |




|
|